The catalytic degradation of polystyrene, carried out in sealed tubes with solid catalysts having different acidic properties (i.e. silica-magnesia, silica-titania, mordenite and two silica-aluminas), was studied. Reaction temperatures in the range 360-420°C for reaction times up to 30 min were investigated. The reaction was followed by ESR analysis through a direct quantitative determination of radicals. The kinetic parameters of the initiation step of the multi-step process of polystyrene degradation were obtained, through a computer optimization routine applied to the experimental data. The results are compared with those obtained for the pure thermal reaction.

Polystyrene thermodegradation IV. Kinetics of radical formation in the presence of solid catalysts / P. Carniti, A. Gervasini, S. Bernardelli. - In: POLYMER DEGRADATION AND STABILITY. - ISSN 0141-3910. - 57:3(1997), pp. 301-306.

Polystyrene thermodegradation IV. Kinetics of radical formation in the presence of solid catalysts

P. Carniti
Primo
;
A. Gervasini
Secondo
;
1997

Abstract

The catalytic degradation of polystyrene, carried out in sealed tubes with solid catalysts having different acidic properties (i.e. silica-magnesia, silica-titania, mordenite and two silica-aluminas), was studied. Reaction temperatures in the range 360-420°C for reaction times up to 30 min were investigated. The reaction was followed by ESR analysis through a direct quantitative determination of radicals. The kinetic parameters of the initiation step of the multi-step process of polystyrene degradation were obtained, through a computer optimization routine applied to the experimental data. The results are compared with those obtained for the pure thermal reaction.
English
Settore CHIM/02 - Chimica Fisica
Articolo
Esperti anonimi
1997
57
3
301
306
Pubblicato
Periodico con rilevanza internazionale
info:eu-repo/semantics/article
Polystyrene thermodegradation IV. Kinetics of radical formation in the presence of solid catalysts / P. Carniti, A. Gervasini, S. Bernardelli. - In: POLYMER DEGRADATION AND STABILITY. - ISSN 0141-3910. - 57:3(1997), pp. 301-306.
none
Prodotti della ricerca::01 - Articolo su periodico
3
262
Article (author)
no
P. Carniti, A. Gervasini, S. Bernardelli
File in questo prodotto:
Non ci sono file associati a questo prodotto.
Pubblicazioni consigliate

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/2434/195513
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus 6
  • ???jsp.display-item.citation.isi??? 6
social impact