Dramatic advances in nanostructured MOFs have been strongly promoted by the introduction and development of new synthetic methods that control the size, morphology, and nano/microstructure. High intensity ultrasound method suggests an environmentally friendly, facile and versatile synthetic method to these nanostructured materials that are complicated to synthesize by commonly used methods. Both Solvothermal and sonochemical methods were used to synthesize the new urea-based metal-organic framework [Cd(L1)(DMF)3] (1). Compound 1 was structurally characterized by using X-ray crystallography and spectroscopically by different techniques. The effect of concentration of the initial reagents, time of sonication and sonication power on size and mor- phology has been studied. The results indicate that decreasing concentration of initial reagents, along with increasing ultrasonic radiation time, cause a dramatic effect on the size and morphology of compound 1. Calcination of the nano-sized plate-like particles of compound 1 at 550 °C under air atmosphere yields CdO nanoparticles.

Ultrasound and solvothermal synthesis of a new urea-based metal-organic framework as a precursor for fabrication of cadmium(II) oxide nanostructures / L. Esrafili, A.A. Tehrani, A. Morsali, L. Carlucci, D.M. Proserpio. - In: INORGANICA CHIMICA ACTA. - ISSN 0020-1693. - 484(2019 Jan 01), pp. 386-393. [10.1016/j.ica.2018.09.025]

Ultrasound and solvothermal synthesis of a new urea-based metal-organic framework as a precursor for fabrication of cadmium(II) oxide nanostructures

L. Carlucci
Penultimo
;
D.M. Proserpio
Ultimo
2019

Abstract

Dramatic advances in nanostructured MOFs have been strongly promoted by the introduction and development of new synthetic methods that control the size, morphology, and nano/microstructure. High intensity ultrasound method suggests an environmentally friendly, facile and versatile synthetic method to these nanostructured materials that are complicated to synthesize by commonly used methods. Both Solvothermal and sonochemical methods were used to synthesize the new urea-based metal-organic framework [Cd(L1)(DMF)3] (1). Compound 1 was structurally characterized by using X-ray crystallography and spectroscopically by different techniques. The effect of concentration of the initial reagents, time of sonication and sonication power on size and mor- phology has been studied. The results indicate that decreasing concentration of initial reagents, along with increasing ultrasonic radiation time, cause a dramatic effect on the size and morphology of compound 1. Calcination of the nano-sized plate-like particles of compound 1 at 550 °C under air atmosphere yields CdO nanoparticles.
Metal-organic framework; Sonochemical; Nano-structure; Hydrogen bonding; Urea group
Settore CHIM/03 - Chimica Generale e Inorganica
   PIANO DI SOSTEGNO ALLA RICERCA 2015-2017 - LINEA 2 "DOTAZIONE ANNUALE PER ATTIVITA' ISTITUZIONALE" (2016)
   UNIVERSITA' DEGLI STUDI DI MILANO
1-gen-2019
21-set-2018
Article (author)
File in questo prodotto:
File Dimensione Formato  
197_2018_ICA_Morsali.pdf

accesso riservato

Tipologia: Publisher's version/PDF
Dimensione 8.17 MB
Formato Adobe PDF
8.17 MB Adobe PDF   Visualizza/Apri   Richiedi una copia
20x_2018_19_ICA_Morsali_ASAP.pdf

Open Access dal 25/09/2020

Tipologia: Post-print, accepted manuscript ecc. (versione accettata dall'editore)
Dimensione 1.86 MB
Formato Adobe PDF
1.86 MB Adobe PDF Visualizza/Apri
Pubblicazioni consigliate

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/2434/593367
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus 27
  • ???jsp.display-item.citation.isi??? 22
social impact