An alternative approach was developed for surface treatment of as-received commercial AA 2024 T3 by using a pyrrole-based silane (SiPy). For film deposition, just one immersion step is enough, followed by curing. SiPy layer structure contains both polysiloxane bonds and pyrrole oligomers, with some degree of doping, giving a highly coherent layer. The superior film quality with respect to simple polysiloxane, is probably the main reason for the better corrosion performance obtained for SiPy on 2024.

Pyrrole-based silane primer for corrosion protection of commercial AA 2024 T3 / M. Trueba, S.P.M. Trasatti. - 38:(2008), pp. 14-26. [10.4028/www.scientific.net/AMR.38.14]

Pyrrole-based silane primer for corrosion protection of commercial AA 2024 T3

M. Trueba
Primo
;
S.P.M. Trasatti
Ultimo
2008

Abstract

An alternative approach was developed for surface treatment of as-received commercial AA 2024 T3 by using a pyrrole-based silane (SiPy). For film deposition, just one immersion step is enough, followed by curing. SiPy layer structure contains both polysiloxane bonds and pyrrole oligomers, with some degree of doping, giving a highly coherent layer. The superior film quality with respect to simple polysiloxane, is probably the main reason for the better corrosion performance obtained for SiPy on 2024.
Al alloys; Polypyrrole; Silanization
Settore ING-IND/23 - Chimica Fisica Applicata
2008
http://www.sciencepress.com/getaccess/61260
Article (author)
File in questo prodotto:
Non ci sono file associati a questo prodotto.
Pubblicazioni consigliate

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/2434/55747
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus 0
  • ???jsp.display-item.citation.isi??? 0
social impact